ABS Fender Liner: 2.5mm Thermoformed Fit

A tier two supplier in Pune had 4 percent of liners returned from the assembly line for a 1.5 mm gap at the arch lip, and another 2 percent cracking at the pushnut holes after a winter trial. The material was correct ABS at 2.0 mm. The abs fender liner had been drawn without draft on the deep section, so the part was released from the tool slightly distorted and the clips then pulled it into place.

Fender liners are a forming discipline more than a material one, and the fix usually sits in the tooling drawing.

Why ABS for an ABS fender liner

ABS gives a good balance here: enough impact strength at -20 C to take a stone, sufficient heat resistance for the radiant heat near a brake disc, and good chemical resistance to road salt and the washer fluid that collects in an arch. At 2.5 mm it holds shape on a 600 mm span without the drumming that a thinner sheet shows at speed.

  • Gauge: 2.0 mm for shallow arch sections; 2.5 mm for deep sections and for liners behind a rear wheel.
  • Draft: 2 degrees minimum on all draw walls, 3 degrees on the deep section.
  • Shrink: 0.6 to 0.8 percent, compensated in the tool, not in the trim.
  • Fixings: 6 mm pushnut holes with a 1 mm land, and a 12 mm washer diameter to spread the load.

The crack at the pushnut hole is a clamp load problem

A pushnut on a 2 mm ABS sheet pulls a 12 mm cone of material. When the liner is distorted, the clip pulls it straight and the hole sees a permanent load that turns into a crack at low temperature. Two fixes: correct the distortion at the tool, and add a 1 mm land around the hole so the washer bears on flat material.

Salt spray is the slow failure. ABS resists chloride well, but a liner that traps salt against the body will corrode the panel behind it. The liner should sit 15 mm clear of the body in the lower arch, so water drains instead of pooling.

Trimming and assembly

A thermoformed liner is trimmed on a five-axis fixture, not hand cut. The lip that meets the wing has a 2 mm tolerance, and hand trimming shows as a wavy edge in the arch gap that customers notice at the dealership.

abs fender liner fitted inside a car wheel arch during assembly

River People supply

River People supplies ABS sheet in 2.0 and 2.5 mm for liner tooling, with gauge held to plus or minus 0.05 mm and a lot certificate for each pallet. Sheet is delivered flat and dry, since ABS absorbs moisture and forms surface streaks if it is not dried before thermoforming.

Send your liner drawing and clip pattern to oversales@rpplexiglass.com for a sheet and forming consultation.

Interior trim uses the same 2 to 3 mm ABS stock, covered in our ABS automotive interior trim guide.

Frequently Asked Questions

Is ABS suitable for a winter climate?

Standard ABS keeps usable impact strength to about -20 C. For markets below that, a high-impact ABS grade is specified, or the liner moved to a PP blend.

Can the liner be painted body colour?

Yes, with an adhesion promoter and a flexible additive in the paint. Unpainted liners are the norm because the arch is not usually visible.

What causes a liner to drum at speed?

A panel with too little stiffness over a large unsupported area, or a missing clip. Adding a rib or one extra fixing point usually removes it without changing gauge.