Acrylic clock face panels are the part of a wall clock that a customer actually reads, and a face that turns milky or picks up a grey cast makes the whole unit look cheap on a wall.
A coffee chain replaced 40 dials in 2019 because the original 3 mm faces had bowed around the centre hole and the hands scraped at the 12 position. The replacement moved to 5 mm with a support plate.
Dial thickness and hand clearance on an acrylic clock face
- Diameter 300 mm: 4 mm, single hand set
- Diameter 500 mm: 5 mm with backing plate
- Diameter 800 mm: 6 mm, movement on a separate bracket
- Hand clearance: 7 mm behind the dial minimum
The dial is a flat plate held at one point by a spindle, so the load case is not impact but sag over years. A backing plate spreads the load and keeps the centre flat, which is what stops hands from scraping.
Print, polish and light in the room
A reverse printed dial keeps the ink behind the acrylic, so a wipe across the face cannot touch the numerals. A face printed on the front is cheaper and shows every scratch from cleaning within a year.
Edge and reflection
Polished edges catch room light and give the dial a bright rim; a sanded edge reads grey and makes the whole face look dull. The reverse print also needs a white backing coat or the numerals turn transparent under bright downlighting.
Cutting and polishing tolerances for dial blanks are set out in acrylic sheet cut to size.
Send your dial diameter, movement type and quantity to oversales@rpplexiglass.com for a quotation.
Frequently Asked Questions
What thickness for a 500 mm clock face?
4 mm up to 400 mm diameter, 6 mm above that. A large face at 4 mm bows under its own weight once the movement is fitted off centre.
Will an acrylic face yellow in a shop window?
Cast acrylic with UV stabiliser holds its clarity far longer than extruded sheet. A face in direct south glazing is the case where the grade matters most.
How is the movement mounted?
On a plate behind the face with a clearance hole through the dial. A movement hung on the face itself marks the print and eventually cracks at the spindle.