Polycarbonate Bus Stop Shelter: Street Glazing

A city transport department replaced 340 polycarbonate bus stop shelter panels in one contract, and the report behind the decision had two findings. Panels on south facing stops had yellowed to a visible tint within five years, and panels that had been struck stayed in the frame but leaked rain at the bottom edge.

Both are detail failures, and both are fixed at specification stage.

UV and the polycarbonate bus stop shelter panel

  • Sheet: 6 mm for a standard stop, 8 mm at interchange stops
  • UV: co extruded cap on the street facing side
  • Coating: hard coat for graffiti and cleaning
  • Frame: captive gasket, 4 mm EPDM, dry glazed
  • Movement: 3 mm clearance per metre, oversize fixing holes
polycarbonate bus stop shelter panel at a city bus stop

A south facing stop in a temperate city takes about twice the UV dose of a north facing one. On mass tinted sheet that difference shows as a visible colour step between two stops on the same street, which is the complaint that reaches a council first.

Vandalism and the polycarbonate bus stop shelter edge

The struck panel rarely fails in the middle. It fails at the bottom edge where a kicked panel meets a rigid channel, and water then enters behind the gasket. A captive frame that holds the pane on all four sides after an impact, with a drained bottom rail, keeps the shelter weathertight until the pane is swapped.

Replacement and the polycarbonate bus stop shelter kit

A municipal crew should be able to change one pane without closing the stop. A pane cut to the frame opening with the gasket pre fitted, packed one per stop with a fixing set, gets the job under an hour. Panes shipped loose, with gaskets in a separate bag, turn a one hour job into a morning.

River People supplies shelter kits cut to your frame with pre fitted gaskets and hard coated faces. Send panel count and maintenance interval to oversales@rpplexiglass.com.

Send the shelter drawing, panel count and city maintenance interval to oversales@rpplexiglass.com for a quotation on a replacement kit per stop.

Shelter glazing with a different frame system is covered in polycarbonate bus shelter glazing.

Frequently Asked Questions

How is graffiti removed?

With a hard coated surface and a solvent wipe. Uncoated polycarbonate absorbs marker pigment and requires mechanical polishing, which hazes the panel.

Why do shelter panels yellow in five years?

Because the UV cap was omitted or the sheet was mass tinted. On a south facing stop the difference is visible side by side within three summers.

What fixing survives an impact?

A captive gasket frame that holds the pane after a strike, rather than a bolt pattern that lets the pane fall clear.