A polycarbonate polytunnel glazing decision is usually made on light transmission, and it is usually the wrong number to open with. Wind uplift at the hoop spacing decides whether the panel is still attached in the third winter.
Both numbers can be checked before a purchase order, and both belong in the same conversation.
Light and the polycarbonate polytunnel glazing
- 8 mm twinwall: 78 percent transmission, clear
- 10 mm twinwall: 74 percent, clear
- Diffused grade: 82 percent scatter, no hot spots
- UV block: 380 nm cut for crop shaping
Film starts near 90 percent and falls to 75 within two seasons as it chalks and sags. Twinwall starts lower and holds its number for a decade. On a lettuce or herb crop the crossover is inside the second year, which is why nurseries with a five year plan move to sheet.
Uplift, hoops and the polycarbonate polytunnel glazing bay
A 1.2 m hoop at a 6 m span carries roughly 60 kg per square metre of uplift in an exposed site, and an 8 mm twinwall fixed on a 100 mm land at each hoop holds that when the fixing is a screw with a sealing washer, not a clip. Clips let the panel flutter, and flutter fatigues the flute wall at the fixing line.
Condensation and the crop
Water drops from a bare inner face land on the canopy and open the door to botrytis. An anti condensation coat, plus a 3 degree slope along the bay, moves the water to the gutter instead. On tomato and soft fruit crops that single detail decides whether the sheet is worth the premium.
River People cuts and caps twinwall to your hoop layout, clear or diffused, with fixing kits and gasket tape. Drawings go to oversales@rpplexiglass.com.
Send your tunnel drawing, hoop spacing and crop type to oversales@rpplexiglass.com for a quotation on cut and capped twinwall panels.
Hoops, spans and fixing detail for roofs are set out in our twinwall greenhouse roof glazing guide.
Frequently Asked Questions
How much light does twinwall lose compared with film?
About 12 to 18 percent against new film. Against film in its second season, which has yellowed and sagged, twinwall is often brighter and stays constant for a decade.
Which thickness for a 6 m span tunnel?
8 mm on 1.2 m hoop spacing, 10 mm where hoops are at 1.5 m or the site is exposed. Thicker panels stiffen the bay and reduce flutter damage.
Does twinwall need a condensation control coat?
On the inner face, yes for crops prone to leaf wetness. An anti condensation coating keeps droplets flowing to the gutter instead of dropping on the canopy.